7591 839 long-acting high-build antifouling coating
+
  • 7591 839 long-acting high-build antifouling coating

7591 839 long-acting high-build antifouling coating

7591 is a high-performance and long-acting non-tin self- polishing antifouling coating composed of acrylic resin as base material,cuprous oxide as main antifouling agent and deep additives, etc, The paint film has excellent antifouling efect and can preventmarine organisms from fouling the ship bottom for a long time. The antifouling period can reach more than 36 months.

Category:

Keywords:

7591 839 long-acting high-build antifouling coating

Product Inquiry:

Product Description

Product introduction

7591 is a high-performance and long-acting non-tin self- polishing antifouling coating composed of acrylic resin as base material,cuprous oxide as main antifouling agent and deep additives, etc, The paint film has excellent antifouling efect and can preventmarine organisms from fouling the ship bottom for a long time. The antifouling period can reach more than 36 months.

 

Recommended applications

It is aenerally used as antifouling coating of marine facilities such as ship bottoms, docks, ofshore platforms, beacons and underwatersteel gates, so as to prevent marine organisms from adhering and fouling.

 

Product information

Appearance:Red and brown

Volume solids:56±3%

Recommended DFT:50-100 μm (corresponding WFT=82 μm)

Theoretical quantity required (40 μm):5.6-11.2 m 2 /L or 2.55-5.1 m 2/kg

SG:2.2 kg/L

Flash point:Above 28°C

 

Construction conditions

The substrate should be clean and dry, and the constructiontemperature should be higher than 3'C above the dew point toavoid condensation.

It is recommended to apply this product at <85%RH.

This product can be applied in <-10°C.

Adequate ventilation is required during drying.

During repairing, clean the residual self-polishing or abrasiveantifouling coating with proper detergent to remove surfacegrease.Then wash thoroughly with high-pressure fresh waterto remove the saponification layer with poor adhesion.

During repairing,the use of sealing paint depends on the typeand conditions of residual antifouling coating.

 

Painting method

Painting methods:Airless spraying

Diluent:102 diluent

Dilution:0-5% of the coating weight, The actual addition may be adjusted according to the field painting method

Nozzle size:0.4-0.5 mm

Spraying pressure:15-30 Mpa

 

Drying time
Temperature 5℃ 10℃ 20℃ 30℃
Surface drying 6h .h 1.5h 1h
Hard drying 36h 30h 24h 16h

 

Repainting interval
Subsequent coats Temperature 5℃ 10℃ 20℃ 30℃
Chlorinated rubberor acrylic acid Shortest 36h 24h 16h 8h
Longest 15d 15d 15d 15d

 

Undock time
Temperature 5℃ 20℃ 30℃
Shortest undocking time 36h 24h 16h
Longest undocking time 15d 15d 15d

 

Film thickness
Docking interval (month) new ship building old ship repair
12 months 100 um X 1 100 um X 1
24 months 100 um X 2 100 um X 2
36 months 100 um X 3 100 um X 3

 

Packing specifications: 21.5kg

Shelf life: 12 months

Safety measures: Refer to our Material Safety Data sheet(MSDs)

 

Disclaimer: The above produtiformatin and data are accumulated acordina to ou experience in experiments and pracicaluse, and can be used as a constuction quideFor painting works that we are not informed, we ony guarantee the qualty ofthe coating itsel,butwe are not responsilble for other problems. We have the righto modify thimanualdue to the continuous improvement of our product.

Recommended Products

Welcome to leave us a message or inquiry.

Our staff will contact you within 24 hours (on business days). If you require any additional services, please feel free to call our service hotline!